When the welding head is not strong or the wire is brought up, the first should be to grind the welding head, not to increase the parameters. When grinding the welding head, be careful not to use too much force to grind, only need to use a grinding disc or W5 Use fine sandpaper to lightly polish the bottom of the welding head with one or two strokes.
There is insulating glue in the middle of the welding head and then loosening it will affect the contact position of the welding heads on both sides, causing the welding effect to be very bad. Therefore, it is strongly recommended that the welding head is installed and used until the welding head can not be used before taking it out. Do not frequently disassemble and assemble the welding head in the middle.
Because the welding uses a large current, the reason that a large parameter is often required is that the center of the welding head clamped by the welding head clamp is very dirty, which seriously affects the flow of current. Therefore, it is recommended to clean the area once a month.
The above is the application method to extend the life of the spot welding head. I hope it can bring you assistance.
Mailbox:brian.he@soucua.com
Mailbox:danny.ng@soucua.com
Mailbox:smion.siew@soucua.com
Mailbox:mila.lin@soucua.com
Postcode:523300
Address:No. 11, Hengjiao Hengling Street, Hengjiao Village, Shijie Town, Dongguan City, Guangdong Province, China
Copyright ©2020Dongguan Soucua Hardware Electronics Co., Ltd.
All Rights Reserved